Home / Materials / Sinterit PA12 Smooth

Sinterit PA12 Smooth

PA12PowderSLSSinterit

Quick answer

Sinterit PA12 Smooth is the standard PA12 powder for Sinterit's Lisa-series desktop SLS printers: 32 MPa tensile strength and 10% elongation at break per Sinterit's powder specification (PN-EN ISO 527-2), with a material refreshing ratio of 22% — the lowest manufacturer refresh figure in this database.

PA12 Smooth is the entry powder of the Sinterit ecosystem — the grade the Lisa and Lisa Pro benchtop SLS printers are specified around. Its headline tensile figures (32 MPa, 10% elongation) sit below the industrial SLS grades in this database, which reflects the desktop machine class it is tested on; Sinterit's own specification notes that final part properties vary with part design and orientation.

The figure that stands out is the refreshing ratio: 22%. Sinterit defines it in the specification exactly as this site does — the percent of fresh powder that has to be mixed with used (unsintered) powder for the next print — and a low ratio is the core of the desktop SLS cost argument, because most of every build is recovered powder.

Properties (manufacturer datasheet)

PropertyValueOrientation / conditionTest standard / note
Tensile strength32 MPaPN-EN ISO 527-2
Elongation at break10 %PN-EN ISO 527-2
Charpy impact strength (unnotched)16 kJ/m²PN-EN ISO 179-1
Further values, as published (ranges & text)
Charpy impact strength (unnotched)16 kJ/m²PN-EN ISO 179-1/1eU:2010, per Sinterit powder specification
Granulation18–90 µmPer Sinterit powder specification

Values are reproduced from the manufacturer source(s) listed below, exactly as published. Properties the manufacturer does not publish are omitted rather than estimated — see the sourcing policy.

Processing notes

Typical applications

Manufacturer, process & related entries

Manufacturer

Sinterit

Poland · Materials & machines

Sinterit is a Polish SLS company based in Kraków, known for the Lisa series of benchtop selective laser sintering printers and its own line of SLS powders. Its PA12 Smooth powder — with a manufacturer refreshing ratio of 22% — is the first Sinterit grade listed in this database.

Official website — sinterit.com

Process

SLS — Selective Laser Sintering

Powder-bed fusion

A laser scans each cross-section over a heated bed of nylon powder, sintering one layer at a time; the surrounding unfused powder supports the part.

Run the numbers for this grade

Two calculators read this database: the part cost estimator prices a part in this grade from its volume and datasheet density, and the refresh ratio calculator plans the virgin-powder blend for a build.

Frequently asked questions

What does Sinterit's 22% refreshing ratio mean?

Per Sinterit's own footnote in the powder specification: the percent of fresh powder that has to be mixed with used (unsintered) powder to be reused in the next print. At 22%, a charge is 22% fresh and 78% recovered powder — a lower virgin share than the 30–50% figures the industrial grades in this database publish.

Why are PA12 Smooth's strength figures lower than EOS PA 2200's?

Different machine class and test setup: PA12 Smooth is specified on Sinterit's Lisa-series desktop printers, PA 2200 on EOS industrial systems. Both are PA12; compare the figures as system-level results (printer + powder + parameters), not as pure polymer rankings.

Which printers run PA12 Smooth?

The specification lists the Lisa & Lisa Pro. Sinterit sells the powder in Starter (first print) and Fresh (refresh) variants of the same grade.